1,Performance parameters of graphite rod
Item | Value |
Resistivity μΩ•m | 8-10 |
C percent | Greater than or equal to 99 |
Ash percent | Less than or equal to 0.1 |
Density g/cm3 | Greater than or equal to 1.8 |
Shore hardness | 55 |
Compressive strength Mpa | Greater than or equal to 90 |
Flexural strength Mpa | Greater than or equal to 40 |
Thermal conductivity W/m.k | 125 |
Coefficient of thermal expansion | 4.8 |
2,Product description
Graphite rod is a non-metallic product, which is made of carbon and graphite with appropriate binder, extruded and baked at 2200 degree . It is commonly used as an electric heater in vacuum furnace. The maximum service temperature can reach 3000 degree . It is easy to oxidize at high temperature. In addition to vacuum, it can only be used in neutral atmosphere and reducing atmosphere. It has small thermal expansion coefficient, large thermal conductivity and high temperature resistance, Excellent cold and heat resistance.
3,Product characteristics
1)Excellent chemical stability and strong resistance to acid and alkali corrosion
2)It has small expansion coefficient, can withstand extreme cold and heat, and is not easy to deform
3)Good conductivity, not easy to break
4)It is easy to oxidize at high temperature. Except for vacuum, it can only be used in neutral and reducing atmosphere.
4,Product application field
metal smelting
Electrolytic plating
Industrial heat treatment
chemical industry
Metalworking
6.Good feedback of product use effect,the products have been exported to South Korea, Oman, the United States, and India.
7.The manufacturer is a professional manufacturer and can provide complete product index test reports or third-party test reports.
Do you want to find a professional supplier of Graphite rod products?
Do you want to find a stable and credible supplier?
Then let's contact with Tairan company
Contact me:
Email:wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / FAX: 86-0533-4188518
Rose: plus 86-13275332819(wechat/whatsapp number)
Issiq teglar: Graphite Rod, China, manufacturers, suppliers, factory, use, property