Graphite Polystyrene Foam Board

Graphite Polystyrene Foam Board

The graphite polystyrene board is added IR absorbing agents and reflection agent,avoid the heat flow caused by radiation. The thermal insulation performance of graphite polystyrene board is improved by 20 percent compared with ordinary EPS material. It is the preferred thermal insulation material.
So'rov yuborish
Hozir chat
Ta'rif

1,product description: the main raw materials for graphite polystyrene board are high purity graphite and polystyrene beads. Polystyrene particles form small black beads with foaming agents, which make them expand after foaming. Graphite polystyrene board is a new generation of thermal insulation material, which does not contain chlorine monomer and is made by more advanced processing technology, which greatly improves the thermal insulation performance of the material.

2,Charactreistic of product

1) Micro closed cell structure, low thermal conductivity and excellent thermal insulation effect

2) The molecular structure of polystyrene does not absorb water. Therefore, the product has excellent water resistance, moisture resistance and impermeability. The volumetric water absorption of the board is less than 1 percent , which is much smaller than that of polyurethane board and general EPS board

3) Good impact resistance. When the density is less than 40kg / m3, the compressive strength can reach 350Kpa

4) Excellent compressive performance, even if immersed in water, does not change, which is not available in other thermal insulation materials

5) Anti corrosion and easy construction

3,Application: building wall, cold storage, ship, thermal insulation vehicle

4,Product performance parameters

Item

Unit

Value

Density

Kg/m3

26-35

Flame resistance


B1

Compressive strength

Kpa

150-350

Thermal conductivity

W/m.k

Less than or equal to 0.030

Water absorption

percent

Less than or equal to 1.5

Dimensional stability

percent

Less than or equal to 2.0

Color


Gray black white

5,Good feedback of product use effect,the products have been exported to South Korea, Japan,Pakistan

6,We are a professional supplier, who can provide customers with free product technology, use and other issues

 

 

 

Do you want to find a professional supplier of Graphite Polystyrene Foam Board?

Do you want to find a stable and credible supplier?

Then please contact with us

 

Contact me:

Email:wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518 

Rose: plus 86-13275332819(wechat/whatsapp number)

 


Issiq teglar: graphite polystyrene foam board, China, manufacturers, suppliers, factory, use, property

So'rov yuborish
Biz bilan bog'lanish
  • Tel: +86-533-4188518}
  • Mob: +8613275332819}
  • E - Pochta: sdwenping@163.com
  • Qo'shish: Xona 711, No.3, Yanhe Yo'l, "Foran", Zibo, Shandong, Xitoy

(0/10)

clearall